OpticalMicroscopySOP
Document ID: HF-QC-MIC-004 Prepared by: Shreeja Gupta Version: 1.0 Date: March 2, 2026
1. Purpose
To inspect patterned wafers using optical microscopy to verify feature quality, alignment, and dimensions after lithography and development.
Supports HackerFab fabrication workflows targeting <10 µm feature sizes using calibrated microscope measurements.
2. Scope
Applies to:
Wafers after development (HF-PROC-DEV-003)
Lithography calibration wafers
Feature size verification and process troubleshooting
3. Responsibilities
Operator: Inspect wafer and record measurements.
Process Lead: Maintain calibration accuracy.
Team Lead: Review results for process improvements.
4. Equipment & Materials
Equipment
Optical microscope (AmScope)
Amscope measurement software
Microscope stage
Cleanroom wipes
Computer for image capture
Materials
Patterned wafer
Calibration slide (µm scale)
5. Safety Precautions
Handle wafers with tweezers only.
Avoid touching lens surfaces.
Do not drop wafers on stage.
Turn off illumination after use.
6. Calibration Requirements
Before measuring feature sizes:
Use a calibration slide with known µm markings.
Calibrate at each magnification level used.
Save calibration settings in software.
7. Procedure
8. Expected Results
Sharp, well-defined patterns.
Feature sizes within the expected range.
Verification of lithography calibration.
9. Troubleshooting
Blurry image
Out of focus
Refocus stage
Wrong feature size
Calibration error
Recalibrate microscope
Uneven patterns
Spin coat issue
Check SC SOP
Overdeveloped pattern
Too long dev time
Adjust DEV SOP
10. Notes
Always recalibrate after changing magnification.
Keep image records for process tracking.
Use microscopy results to tune exposure dose and spin speed.
11. Revision History
1.0
March 2, 2026
Initial draft