> For the complete documentation index, see [llms.txt](https://docs.hackerfab.org/home/llms.txt). Markdown versions of documentation pages are available by appending `.md` to page URLs; this page is available as [Markdown](https://docs.hackerfab.org/home/fab-toolkit/tube-furnace/malfunction-log.md). Agents can also search and read this documentation through its [MCP server](https://docs.hackerfab.org/home/~gitbook/mcp).

# Malfunction Log

7/3 - Furnace 5 kanthal wire double twisted fried, had to reattached ceramic wire

<br>

7/14 - Furnace 5 ceramic wires fried, first attempt after previous repair, was running for 3+ hours

<br>

| Thermocouple side                                                                                                                                                                                                     | Entry Side                                                                                                                                                                                                            |
| --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- | --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- |
| ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2Faz49oJECjdj0yNK52CKa%2Funknown.png?alt=media\&token=145f953e-b9ed-4b8b-9a27-aa2e01973864) | ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2FzdowVe2dS1u1mNd0QfuW%2Funknown.png?alt=media\&token=167f0823-ca1e-4d80-b770-3c6f629436f2) |

<br>

Furnace 6 ceramic wires fried, first attempt, ran for 20+ minutes

<br>

| Thermocouple side                                                                                                                                                                                                     | Entry Side                                                                                                                                                                                                            |
| --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- | --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- |
| ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2FbHd6fkD2BScUdZxSAISV%2Funknown.png?alt=media\&token=8ade645f-1331-429f-ace7-9494c5c6f825) | ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2Fq7z3ZxQmuL1OQzCdTeDK%2Funknown.png?alt=media\&token=541e6ea9-0a7c-488c-b5c8-59c28a9387f5) |

<br>

Ceramic coating on both furnaces was disintegrating where wires had contact

<br>

Ceramic beads seem a little burnt but otherwise intact, Furnace 5 and 6 each had one ceramic wire still in contact with kanthal, being held together with bead despite being fried → possible only the thermocouple wire side was completely fried through, however it’s clear that both wires are under severe heat stress during operation

\
\ <br>

7/15 - Discovered kanthal wire coil on furnace 6 had been burned and rusted through

<br>

To combat this, next tube was made with as few kinks in wiring as possible, and the kanthal wire is used as the connector to the motor control as opposed to ceramic coated copper

| ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2FSOD7ITUhIOzQLtZyVfJM%2Funknown.png?alt=media\&token=b72f0660-40f6-457b-a83f-ad6c3afd859d) | ![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2FAQieWT5ilYAZm9YsrWpL%2Funknown.png?alt=media\&token=d6509093-ed53-4992-8598-908ab975eb7c) |
| --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- | --------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- |

<br>

8/25 - Since switching wiring to full kanthal and using one solid piece of wire, shorts have been discovered in the machines after repeated use. Found out the cause was due to the weave casing of wiring was being shredded through

<br>

9/8 - Incorporating the PID controller with a lack of motor control results in too much current being drawn and the kanthal wires becoming so hot they burn through the insulation weave

![](https://2353182699-files.gitbook.io/~/files/v0/b/gitbook-x-prod.appspot.com/o/spaces%2FXgXjz6D0Vz2o0EOp8JO5%2Fuploads%2FGF9PqqXfMh3w9y24rqO3%2Fimage.png?alt=media\&token=81a50d32-476b-4ab9-8566-e7bc4355b250)<br>

9/9 - Incorporated motor control into PID wiring to control current, but creates a problem where current is not being drawn unless an additional element, such as a lightbulb, is incorporated to trick the system into powering on

<br>


---

# Agent Instructions
This documentation is published with GitBook. GitBook is the documentation platform designed so that both humans and AI agents can read, navigate, and reason over technical content effectively. Learn more at gitbook.com.

## Querying This Documentation
If you need additional information that is not directly available in this page, you can query the documentation by asking a question.

Perform an HTTP GET request on the following URL with the `ask` and `goal` query parameters:

```
GET https://docs.hackerfab.org/home/fab-toolkit/tube-furnace/malfunction-log.md?ask=<question>&goal=<user_goal>
```

`ask` is the immediate question: it should be specific, self-contained, and written in natural language.
`goal` is what the user is ultimately trying to achieve, the reason they need the answer. Sharing it helps GitBook give you a better, more relevant answer. A goal is most helpful when it describes the outcome the user wants rather than restating the question. For example, with `ask=how do I create an API token`, a goal like `automate deployments from our CI pipeline` lets GitBook tailor the answer to that use case.

The response will contain a direct answer to the question and relevant excerpts and sources from the documentation.

Use this mechanism when the answer is not explicitly present in the current page, you need clarification or additional context, or you want to retrieve related documentation sections.