Case Western Reserve University

Hacker Fab @CWRU

The Hacker Fab @CWRU is a student-ran lab operating within the Materials for Opto/Electronics Research and Education (MORE) Center. Our goal is to build low-cost and accessible nanofabrication tools. Beyond equipment, CWRU focuses on digital and logic design through Tiny Tapeout.

Current Fab Capabilities:

  • DIY Lithography Stepper

  • Maasi Spincoater

  • Tube Furnace

Projects in Progress:

  • DIY RF Magnetron Sputterer

  • Tiny Tapeout

Core Team:

  • PhD Physics, Andrew Lininger — Supervisor

  • Andrew Csanady — Organization Lead

  • Pieter Verbeek — Vice Lead

  • Kevin Harris — Technical Lead, Lithostepper Lead

  • Davis Bauchner — Magnetron Sputterer Lead

  • J.P. Magbitang — Tiny Tapeout / Logic Design Lead

Contact:

Last updated