Processes
✨
Self Aligned NMOS
November 2023 Update
*NEED TO UPDATE* Microscope Image of Single NMOS Exposure - November 2023
Device Type
NMOS
Gate:
2μm
# of Transistors:
UPDATE
IV Curves of Good NMOS Transistor November 2023. Red is Gate Leakage
NAND Gate
Enhancement Mode NMOS Inverter