Automating our existing spin coater whilst integrating heating and liquid dispensing systems.
Footprint (cm³)
35 x 35 x 50
L x W x H
Reliability (%)
99%
Amount of chips sucessfully processed
Clearance (cm)
15
Room for users to access chips
Heating (°C)
100
Internal Temperature (°C)
+15
Temp. above Room Temp.
Dispense Time (sec)
2
Time per drop dispensed
Open/Close Time (sec)
10
Time taken to open/close lid
Automating the Lab Process
Lab Auto's goal is to automate the steps of the NMOS process for Hacker Fab. This will take the form of a lab robot with integrated machines for each step of the process. Currently, we're focusing on an automated spin coater that will receive a blank chip and spin on HMDS and photoresist, with liquid dispensing and baking capabilities.