Weekly Updates for Shagun Maheshwari (CMOS Project)
Progress tracker: https://github.com/orgs/hacker-fab/projects/34/views/1
Progress Update:
Successfully used the Keithley 4200 to conduct CV tests for the fabed p-type MOSCap. https://docs.hackerfab.org/home/standard-operating-procedures/probe-station-sop
Ran high and low frequency CV tests and compared it to target CV curves for the accumulation, depletion, and inversion regions for a p-type MOSCap. Stored the data for 4 patterns on the chip
Debugged the Keithley 4200 controls
Read/skimmed through the Keithley 4200 CV test manual https://download.tek.com/document/4200%20CV%20ApplicationsGuide.pdf
Watched Sam Zeloof's CV testing video https://www.youtube.com/watch?v=v6Mb7J6c6og
Read through these two documents on CV testing Sam Zeloof linked
Did a code walkthrough with Cesely for the diffusion model and loaded/ran it in google colab https://colab.research.google.com/drive/1cJ8WHxEa8jF9vQnLNw5twRnWye24PjPx
Roadblocks:
Chatted with Cesely and she mentioned it may not make sense to edit the diffusion model code and use that to inform fabing the next set of chips as it is not accurate + a lot of assumptions were made in that model. Her suggestion was to just go ahead with fabing the next set of chips, conduct CV tests, and use those results to inform the parameter changes within the diffusion model. Beleive Jay, Cesely, and I would need to align on this path.
Next Steps:
Work on first presentation for Hacker Fab
Analyze results from the CV tests
Create fabublocks for next set of chips to be fabed
Start fabing next set of chips
Feedback
• Cesely Great job on getting your first set of results from a chip! Do you have these results documented, and have you started interpreting them? It's important to begin analyzing your data as soon as possible, as this will be crucial for your presentation and will also help guide the next set of chip fabrications.
Next Steps for CV Testing: One key aspect I want to determine from the CV testing is whether we can back-calculate carrier concentration and junction depth. These parameters will be essential for refining our understanding of the device characteristics.
Future Experiments & Model Refinement: For the next batch of chips, I suggest performing SOG diffusion while varying the drive-in diffusion parameters, specifically time and temperature. The goal is to use these variations to improve the accuracy of the current model. I have concerns about the reliability of my model due to the assumptions and experimental methods used for verification, so updating it with more accurate CV data is a priority.
Action Items: 1. Outline an experimental plan detailing how you will use CV characterization to refine the model. 2. Identify which parameters you will vary and how this will contribute to improving the accuracy of the model. 3. Once the model is updated, we can use it to make informed predictions for optimal doping levels in n-well and CMOS processes.
Jay
talked with Cesely to clarify, but absolutley use her code from last semester. You need to do this in order to figure out what doping parameters to use when making MOSCaps. The point is to use the model to get close to the desired doping parameters, then test with moscaps, then tune the model, then re iterate on moscap testing with updated model to finalize CMOS doping parameters.
use ceselys model to determine what doping parameters you will use for the first set of moscaps, then fab them this week to stay on schedule.
Progress Update:
Fabricated a p-type MOScap
Completed oxide growth
Completed aluminium evaporation
Created patterns
Patterned
Applied photoresist
Figured out correct procedure for aluminum etching
Learned and used the probe station to see if there was ohmic contact and optimized the aluminum etching process accordingly
HF etched the oxide
Aluminum evaporated again with new pattern
Roadblocks:
Main roadblock was the long time it took to fabricate and improving the aluminum etching process
Also had an issue with the evaporator on the second round of aluminum evaporation where the pressure wouldn't drop below 1e-4 hPa
Next Steps:
Learn more about CV testing and the procedure we want to follow + understand how to interpret the different results we could see and what that tells us about the device
• From Cesely
Good work getting a MOSCap fabricated. This week we should perform a CV test on the chip and seeing if we can get the dopant concentration vs. depth and using this to compare with the model I had from last semester. We should also begin fabricating/developing a process to fabricate MOSCaps more akin to the CMOS process we hope to generate.
Also, it is not clear to me which chips you have fabricated. Did you fabricate a chip with or without the RCA clean? Or both? If you only fabricated one chip, then variations in the Al deposition might affect our observed CV results between chips and may not be related to the RCA clean.
Issues with the Al evaporator are likely caused by the chamber not being clean, since it was used this week for labs.
From Jay
Please make sure to link to the notes/documentation form the fabbing process, ie pics of surface between steps, notes of errors, new findings (like Al etch rate witht eh new ethcant) etc.
Make sure task tracker is updated (as per the update rubric)
Good job working hard to get a clean moscap fabed and working through difficulties of microfabrication
Next steps is a little lacking I would rec
perform CV testing on fabed p type moscap
Interpret results to attain threshhold voltage, flatband voltage, and dopant profile vs depth.
determine doping process for CMOS represntative MOSCaps to be used based on Cesely's code from F24, and make relevant SOPs
Begin fabing of CMOS representative MOSCaps (this may be out of scope for the next week)
BTW I have the new tubes and push rod for the tube furnace
Progress Update:
Did research on performing an RCA clean and wrote the SOP of the RCA clean we will conduct here: https://docs.google.com/document/d/1EJc17dcLvwOp3yGAgUv3rpoIKi2gON022oEVz9VkTkE/edit?usp=sharing
Added initial notes for RCA clean to the CMOS process dev master doc: https://docs.google.com/document/d/1566Sux3ALGOfexcq4ajqJ6XRDOvNgEnyw1Al20tyuYY/edit?tab=t.0
Built a FabuBlocks process for the p-type MOScap fabrication here + got feedback from Cesely : https://www.fabublox.com/process-editor/b12fd11e-5a87-4d3f-ad97-d2f436606290
Created the solutions for SC-1 and SC-2 we will be using for the RCA clean within the fume hood
Completed phase 1 of the Resistor lab
Got HF training done
Got Evaporator training done
Got Fume Hood training done
Roadblocks:
No current roadblocks, tube furnace seemed to have died so couldn't make the p-type MOScap last week but it seems to have been fixed so I can do that next week
Plans:
Conduct an RCA clean following my SOP
Fab a p-type MOScap
Read through chapters 4 and 5 of Modern Semiconductor devices for Integrated circuits again in detail and read through dopant profiles to help with CV testing.
From Cesely
Great work this week! Your documentation looks very good and professional.
It will be imperative that you start fabricating this week as you learned last week things in the lab can take much longer than expected.
How do you intend to measure the effectiveness of the RCA clean? Will you be comparing the results of the RCA clean by having a baseline chip with no RCA clean?
Also, will need to make patterns for your MOS Caps. I can review how to do this with you.
From Jay
Good job getting familiar with the fume hoof and setting up the RCA clean.
I gave feedback on fabublox process via discord, but here is what I recommended instead (to ensure we have a surface bulk contact that can be used for testing MOSCaps doped wells too): https://www.fabublox.com/process-editor/4f8374e9-d89c-4486-b54f-716cac33802e
Progress Update:
Read through chapters 4 and 5 of Modern Semiconductor devices for Integrated circuits
Did research on CV characterization
Wrote the Project Proposal for PMOS including Junction Depth and CV characterization
Completed pattern training with Jay
Roadblocks:
No major roadblocks to report
Plans:
Fab a p-type substrate
Look more into the specific experiments we should conduct for CV characterization
Lab next week
From Jay
Critiques: For the progress update, be sure to link to the document(s) that show evidence of your progress. this week that would be a link to you project proposal
For roadblocks, this is an opportunity to request help, or clarify what you need from us to keep moving forward. I would argue training on certain equipment to be roadblock for you.
For plans, there should be more detail in how you're going to proceed, or link to your working doc that demonstrates your plans in more detail. For example, Fabing a p type MOSCap will require designing a fabublox process and reviewing it with someone, creating the patterns you're going to use for lithography, etc.
For CV testing, I understand you will research specific experiments we what to do, but you should include a tentative plan of what readings youre going to look at first. This can help us guide your research more concretely.
Overall good job!
From Cesely
Great work this week. I would continue to understand and devise a plant to extract specifically the carrier concentration vs junction depth. Also, this week you should begin to fabricate MOS Caps with a p-type substrate. This will be tentative as we are waiting for a power supply for the Thermal Evaporator. In the meantime you should use Fabublox (link below) to create a fabrication process for the MOS Cap.
Progress Updates
Reviewed some documentation from the Project Primer
Had initial group meeting with the CMOS team to go over problems
Read through assigned readings
Roadblocks
No major roadblocks to report
Plans
Read through chapter 1,4,5,6 in the Modern Semiconductor Devices for Integrated circuits textbook
Read through the documents from the Project Primer
Draft project proposal (due Thursday before class)